49 C.F.R. § 179.300-7
Materials.
Cite as 49 C.F.R. § 179.300-7 (2026)
(a) Steel plate material used to fabricate tanks must conform with the following specifications with the indicated minimum tensile strength and elongation in the welded condition. However, the maximum allowable carbon content for carbon steel must not exceed 0.31 percent, although the individual ASTM specification may allow for a greater amount of carbon. The plates may be clad with other approved materials:
Specifications
2
Tensile strength (psi) welded condition
1
(minimum)
Elongation in 2 inches (percent) welded condition
1
(longitudinal) (minimum)
ASTM A 240/A 240M type 304
75,000
25
ASTM A 240/A 240M type 304L
70,000
25
ASTM A 240/A 240M type 316
75,000
25
ASTM A 240/A 240M type 316L
70,000
25
ASTM A 240/A 240M type 321
75,000
25
ASTM A 285 Gr. A
45,000
29
ASTM A 285 Gr. B
50,000
20
ASTM A 285 Gr. C
55,000
20
ASTM A 515/A 515M Gr. 65
65,000
20
ASTM A 515/A 515M Gr. 70
70,000
20
ASTM A 516/A 516M Gr. 70
70,000
20
1
Maximum stresses to be used in calculations.
2
These specifications are incorporated by reference (IBR, see § 171.7 of this subchapter.)
(b) [Reserved]
(c) All plates must have their heat number and the name or brand of the manufacturer legibly stamped on them at the rolling mill.
[Amdt. 179-10, 36 FR 21355, Nov. 6, 1971, as amended by Amdt. 179-42, 54 FR 38798, Sept. 20, 1989; Amdt. 179-43, 55 FR 27642, July 5, 1990; Amdt. 179-52, 61 FR 28682, June 5, 1996; Amdt. 179-52, 61 FR 50255, Sept. 25, 1996; Amdt. 179-53, 61 FR 51342, Oct. 1, 1996; 68 FR 75763, Dec. 31, 2003]