LAC 43:XIII.1715

LAC 43:XIII.1715. Wrinkle Bends in Steel Pipe [49 CFR 192.315]

Last amended: 2004Year: 2026Length: 138 wordsOfficial source

Cite as La. Admin. Code tit. 43, pt. XIII, § 1715

A. A wrinkle bend may not be made on steel pipe to be operated at a pressure that produces a hoop stress of 30 percent, or more, of SMYS. [49 CFR 192.315(a)] B. Each wrinkle bend on steel pipe must comply with the following. [49 CFR 192.315(b)] 1. The bend must not have any sharp kinks. [49 CFR 192.315(b)(1)] 2. When measured along the crotch of the bend, the wrinkles must be a distance of at least one pipe diameter. [49 CFR 192.315(b)(2)] 3. On pipe 16 inches (406 millimeters) or larger in diameter, the bend may not have a deflection of more than 1 1/2º for each wrinkle. [49 CFR 192.315(b)(3)] 4. On pipe containing a longitudinal weld the longitudinal seam must be as near as practicable to the neutral axis of the bend. [49 CFR 192.315(b)(4)]