ARSD 61:08:09:44

ARSD 61:08:09:44. Repair of defects

Last amended: 1997Year: 2026Length: 53 wordsOfficial source

Cite as S.D. Admin. R. 61:08:09:44

Defects such as a crack in a welded joint or deep pitting must be completely removed before repair. If the defect penetrates the full thickness of the material, the repair must be made with a complete penetration weld such as a double butt weld or a single butt weld, with or without backing.